MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Blue River Coatings Hyfro-Flex II PIR (Heat Reflective) Polyurethane Top Coat
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is a high performance, heat reflective, single component water dispersible polyurethane. HYDRO-FLEX II PIR is formulated with heat reflective pigments and adhesion promoting additives to provide the option of painting vinyl and plastic substrates with dark colors that minimize heat gain. The product provides outstanding coverage, excellent durability and is easy to apply. HYDRO-FLEX II PIR is a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state agencies for proper handling and disposal.

Characteristics:

  • Excellent adhesion on most plastic substrates to include vinyl, PVC and fiberglass
  • Excellent exterior durability
  • Excellent heat reflective properties
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent linear flexibility
  • Non-photochemically reactive
  • Full gloss-80-85% at 60° glossometer
  • Available in satin to gloss finish
  • Coatings can be applied in a wide range of temperature and humidity without the use of retarders
  • Water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • No discoloration or loss of flexibility when oven baked (250°F for one hour)
  • Wide range of colors to include metallics
  • Shelf life of 1 year
  • Single component product-unused paint can be returned to container
  • Non-Flammable

    Uses

  • Fiberglass
  • Metal
  • Rigid Vinyl
  • Most Plastics
  • Wood
  • PVC
  • Foam or Cellular PVC
  • Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.05 g/cc1.05 g/cc
    Density 1.05 g/cc0.0378 lb/in³
    Solids Content 37 - 41 %37 - 41 %by volume
     40 - 44 %40 - 44 %by weight
    Volatile Organic Compounds (VOC) Content 188 g/l188 g/l
     
    Mechanical PropertiesMetricEnglishComments
    Impact Test 20.3 J15.0 ft-lbForward and Reverse
    Taber Abrasion, mg/1000 Cycles 100100CS17 wheel, 1000 g load
     
    Thermal PropertiesMetricEnglishComments
    Boiling Point 171 °C340 °F
    Flash Point 79.4 °C175 °F
     
    Processing PropertiesMetricEnglishComments
    Cure Time  10.0 min
    @Temperature 75.0 °C
    0.167 hour
    @Temperature 167 °F
    Recoat, at 50% humidity
     19.8 min
    @Temperature 75.0 °C
    0.330 hour
    @Temperature 167 °F
    Dust Free, at 50% humidity
     45.0 min
    @Temperature 75.0 °C
    0.750 hour
    @Temperature 167 °F
    Dry to handle, at 50% humidity and 75°C
    Shelf Life 12.0 Month12.0 Month
     
    Descriptive Properties
    Evaporation rateSlower than ether
    Flexibility1/8" conical mandrel
    Pencil HardnessHB Minimum
    Solvent Resistancelacquer thinner, acetone, MEK, gasoline, xylene-50 double rubs with saturated cloth.
    Theoretical Coverage665 ft2 at 1 mil
    Vapor DensityHeavier than air

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    BCC Products MB 1200 Polyurethane Foam Modeling Board
    Covestro Baynat® 3002 Polyurethane Foam
    Blue River Coatings Hyfro-Flex Polyurethane Top Coat
    Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 20 pcf
    Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System

    WBLUER09 / 74608

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.