MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 GF 35 1 natural PA 6.6 Conditioned, 35% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Description: AKROMID A3 GF 35 1 natural is a 35% glass fiber reinforced, heat stabilized polyamide 6.6 with high rigidity and strength, UL listed. Applications are mainly component in mechanical engineering and in the automotive industry.

Additive: Heat Stabilizer

Features:

  • High Stiffness
  • High Strength
  • Heat Stabilized
Uses:
  • Automotive Applications
  • Engineering Parts

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Filler Content 35 %35 %ISO 1172
Moisture Absorption 1.8 - 2.0 %
@Temperature 70.0 °C
1.8 - 2.0 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 4.7 - 5.3 %4.7 - 5.3 %ISO 62
Linear Mold Shrinkage, Flow 0.0017 cm/cm0.0017 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0013 cm/cm0.0013 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi5 [mm/min]; ISO 527-2
Elongation at Break 5.0 %5.0 %5 [mm/min]; ISO 527-2
Tensile Modulus 8.40 GPa1220 ksi1 [mm/min]; ISO 527-2
Flexural Strength 245 MPa35500 psi2 [mm/min]; ISO 178
Flexural Modulus 8.00 GPa1160 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 40 1 natural (2381) PA 6.6 Conditioned, 40% Glass Filled, Heat Stabilized
Akro-Plastic Akromid® A3 GF 30 1 natural PA 6.6 Conditioned, 30% Glass Filled
Akro-Plastic Akromid® A3 GF 25 1 natural PA 6.6 Conditioned, 25% Glass Filled, Heat Stabilized
BASF Capron® GR630 HS 30% Glass-Filled Nylon 66 (Conditioned)
Arkema Orgalloy® RS 6620 NAT Polyamide 6.6 Alloy 20% Glass Fiber reinforced

PAKRO206 / 182793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.