MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electronic parts, OA machines, toys and others that require transparency and high impact strength. An Izod impact strength or falling dart impact strength of LG transparent ABS is relatively similar to that of general ABS, it is not easily cracked like SAN or PMMA resin in the condition of low impact energy. TR-557 series is good for applications requiring high impact strength.

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Index of Compound 20 g/10 min20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength at Break 41.19 MPa5974 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Flexural Strength 63.74 MPa9245 psiASTM D790
Flexural Modulus 1.99 GPa289 ksiASTM D790
Izod Impact, Notched 1.471 J/cm2.756 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °FHeat deflection temperature, load unknown; ASTM D648
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %
Transmission, Visible 89.5 %89.5 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 200 °C374 - 392 °FExtrusion cylinder temperature, C1
 210 - 225 °C410 - 437 °FExtrusion cylinder temperature, C2
 230 - 240 °C446 - 464 °FExtrusion cylinder temperature, C3
 240 - 250 °C464 - 482 °FExtrusion cylinder temperature, C4 and C5
Rear Barrel Temperature 190 - 200 °C374 - 392 °F
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Front Barrel Temperature 210 - 230 °C410 - 446 °F
Nozzle Temperature 210 - 230 °C410 - 446 °F
Adapter Temperature 235 - 245 °C455 - 473 °F
Die Temperature 113 - 118 °C235 - 245 °F
Melt Temperature 220 - 240 °C428 - 464 °FInjection molding
 255 - 260 °C491 - 500 °FExtrusion
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Roll Temperature 75.0 - 85.0 °C167 - 185 °FBottom
 80.0 - 90.0 °C176 - 194 °FMiddle
 85.0 - 95.0 °C185 - 203 °FTop
Injection Pressure 68.65 - 88.26 MPa9957 - 12800 psiSecond
 58.84 - 98.1 MPa8534 - 14200 psiFirst
Back Pressure 0.490 - 1.96 MPa71.1 - 284 psi
Screw Speed 50 - 100 rpm50 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
LG Chemical AF342F ABS, Flame Retardant, High Flow
LG Chemical HI100H ABS, High Impact, High Toughness
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding
Chi Mei Polylac® PA-757 ABS

PLGCHEM177 / 50998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.