MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Clariant Acrylonitrile Butadiene Styrene Black 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Clariant Acrylonitrile Butadiene Styrene (ABS) 3D printer filament is made of a high quality and good flowing ABS combined with Clariant additives and pigments to ensure high material performance, end use stability and outstanding color.

General properties:

  • Strong impact resistance
  • High toughness and durability
  • Strong heat resistance
  • High tensile strength
Optimized benefits:
  • Improved lubricity for better printability
  • Reduced thermo-oxidative degradation
  • Minimized undesired yellowing due to ultraviolet radiation
Applications:
  • Mechanical and technical application parts
  • Models
  • Prototypes

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.049 g/cc0.03790 lb/in³ISO 1183
Melt Flow  3.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.7 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
32 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.0 - 44.0 MPa5950 - 6380 psiInjection molded, 50 mm/min; ISO 527
Tensile Strength, Yield 41.0 MPa5950 psiInjection molded, 50 mm/min; ISO 527
Elongation at Break 6.0 %6.0 %Injection molded, 50 mm/min; ISO 527
Modulus of Elasticity 2.34 GPa339 ksiInjection molded, 1 mm/min; ISO 527
Izod Impact, Notched (ISO) 64.0 kJ/m²30.5 ft-lb/in²Injection molded; ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °FInjection molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 72.0 - 79.0 °C162 - 174 °FInjection molded; ISO 75
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 240 °C446 - 464 °FPrint Temperature
 
Descriptive Properties
Bed AdhesionPET or Polyimide tape surface coated with a mixture of ABS dissolved in Acetone or directly onto a PEI surface
Bed Temperatureideally heated up to 110°C and ideally in an enclosed chamber to minimize warping
Fan Settingslow to medium
Print Speed30-50 mm/s
Volume5.6 cm3ISO 1183

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Essentium High Performance PLA Additive Manufacturing Filament
Clariant Polylactic Acid Black 3D Printer Filament
Clariant Polycarbonate + ABS Red 3D Printer Filament
Clariant Natural Color Acrylonitrile Butadiene Styrene 3D Printer Filament
Clariant Polycarbonate + ABS White 3D Printer Filament

PCLAR00010 / 232087

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.