MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elisto THERMOSTAR® 4000 Mold Insulation Material
Categories: Other Engineering Material

Material Notes: Insulation of clamping plates

Information provided by elisto

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 250 MPa
@Temperature 23.0 °C
36300 psi
@Temperature 73.4 °F
Compressive Strength  120 MPa
@Temperature 200 °C
17400 psi
@Temperature 392 °F
 340 MPa
@Temperature 23.0 °C
49300 psi
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 210 °C410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elisto THERMOSTAR® LC 6000 Insulation Material
Brandenburger S 4000 Thermal Insulation Board
Brandenburger GL-P Thermal Insulation Board
Elisto THERMOSTAR® XPS Mold Insulation Material
Elisto THERMOSTAR® LD 500 Frame Press Insulation Material

PELIST001 / 83963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.