MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M TMW Tubing
Categories: Polymer; Thermoset

Material Notes: 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C the adhesive inner wall of the tubing is softened and forced by the shrinking action of the outer wall into contact with all underlying surfaces and small voids. The adhesive forms a flexible bond with a wide variety of rubber, plastics and metals. Upon cooling, 3M TMW tubing provides a tough, protective and insulating barrier, highly resistant to penetration by moisture, chemicals and solvents. #M TMW tubing is rated for continuous operation at temperatures fro -55°C to 110°C and will withstand higher operating temperatures for brief periods. Adhesive reflow will occur at temperatures above 80°C.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Water Absorption 0.10 %0.10 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 4.14 MPa>= 600 psiGasoline Resistance
 6.89 MPa999 psiSolvent Resistance
 17.2 MPa2490 psi
Elongation at Break 400 %400 %
 175 %
@Treatment Temp. 175 °C,
Time 1.21e+6 sec
175 %
@Treatment Temp. 347 °F,
Time 336 hour
Heat Aged
2% Secant Modulus 0.221 GPa32.0 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 15.7 kV/mm400 kV/inSolvent Resistance
 23.6 kV/mm600 kV/inFluid Resistance
 35.4 kV/mm900 kV/in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M MW Heat Shrink Tubing
3M MDT Tubing
3M HDT Heat Shrink Tubing
3M SMS Heat Shrink Tubing
3M Scotch® FP-301 Heat Shrink Tubing

PMM35205 / 169952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.