MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Touchstone CFOAM® 30 Structural Carbon Foam
Categories: Carbon; Other Engineering Material; Composite Core Material

Material Notes: CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally insulating or conducting and whose electrical conductivity can be varied over seven orders of magnitude. It can be fabricated in a variety of shapes, sizes, and densities to meet the property requirements of specific applications.

These foams will not off-gas at elevated temperatures and will not support ignition. Unlike most metals and ceramics, CFOAM mechanical properties do not deteriorate with increased temperature if protected from oxidization, making carbon foams an attractive thermal protection material. Carbon foams also are tolerant to impact damage and can be repaired in-place using carbonaceous adhesives. They can be bonded easily to dissimilar materials, such as metals or PMCs, for oxidation or further impact protection, respectively.

Results from ASTM E1354, ASTM E1515, MIL-STD-1623, Coast Guard IMO, and FTP Code Part I and Part III indicate that CFOAM will pass all key fire tests including radiant panel, smoke generation, toxicity, cone calorimeter, fire resistance, and room corner tests.

Information provided by Touchstone Research Laboratory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.481 g/cc0.0174 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 4.62 MPa>= 670 psiASTM C297
Tensile Modulus 0.827 GPa120 ksiASTM C297
Compressive Strength >= 22.1 MPa>= 3200 psiASTM D365
Compressive Modulus 0.827 GPa120 ksiASTM D365
Shear Strength >= 2.07 MPa>= 300 psiTorsional Shear
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0510 ohm-cm0.0510 ohm-cmStandard
 0.00250 - 2.50e+6 ohm-cm0.00250 - 2.50e+6 ohm-cmTailorable; ASTM D4496
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.04 µm/m-°C2.80 µin/in-°F
Thermal Conductivity 0.300 W/m-K
@Temperature 23.0 °C
2.08 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
Maximum Service Temperature, Air >= 299 °C>= 570 °F
Maximum Service Temperature, Inert >= 3000 °C>= 5430 °F
 
Descriptive Properties
Fire ResistanceISO 1182, ASTM E1354, ASTM E119, IMO FTP Cote Pt. I & III, UL1709Pass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Touchstone CFOAM® 25 Structural Carbon Foam
Touchstone CFOAM® 17 Structural Carbon Foam
Cymat A35620SC 020SS Stabilized Aluminum Foam
Armacell ArmaFORM® FR150 PET foam core
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam

ETOUCH01B / 161707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.