MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU
Categories: Polymer; Thermoplastic; Polyester, TP; Polyurethane, TP

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Seal Grade TPU Products: These products were specially developed for manufacturing hydraulic gaskets or any other heavy-duty application requiring high compression resistance even at high temperature and/or in contact with oils and fats. Two products based on polycaprolactone polyester, E 2202-95A and E 107-93A, and one based on PTMG polyether, E 2203-93A.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ASTM D2240
Tensile Strength, Yield 61.2 MPa8880 psiASTM D412
Elongation at Break 430 %430 %ASTM D412
50% Modulus 10.1 MPa
@Strain 50 %
10.1 MPa
@Strain 50 %
ASTM D412
100% Modulus 13.3 MPa
@Strain 100 %
1930 psi
@Strain 100 %
ASTM D412
300% Modulus 37.4 MPa
@Strain 300 %
5420 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.0620 GPa8.99 ksiASTM D790
Tear Strength 105 kN/m599 pliASTM D624
Abrasion 3535mm3, Abrasion Loss; DIN 53516
Compression Set 26 %
@Temperature 70.0 °C
26 %
@Temperature 158 °F
Method B, 22 hours; ASTM D395
 17 %
@Temperature 23.0 °C,
Time 252000 sec
17 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 154 °C309 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR107-93A Seal Grade TPU
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU
C.O.I.M. LARIPUR® LPR2102-85AE Polycaprolactone Ester Polyurethane
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer

PCOIM035 / 28638

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.