MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baybond® PU 130 Polyurethane Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Baybond PU 130 is an a anionic/non-ionic polyether polyurethane resin dispersed in water.

Properties / Applications: Baybond PU 130 is commonly used as the film- forming component in glass fiber sizing, and is useful for the sizing of glass fibers used to reinforce thermoplastics, especially polyamide. Glass fiber sizes based on Baybond PU 130 have excellent film- forming properties and adhesion. This product also exhibits very good colorfastness at high temperatures and is also highly resistant to hydrolysis. Full mechanical properties of Baybond PU 130 are developed by post-crosslinking for 20 minutes at 170°C. As with any product, use of Baybond PU 130 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Volatiles 70 %70 %
Particle Size 250 - 500 µm250 - 500 µm
pH 7.0 - 8.57.0 - 8.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baybond® PU 401 A Polyester Urethane Polymer
Covestro Baybond® PU 330 Polyester Urethane Polymer
Covestro Baybond® PU 402 A Polyester Urethane Polymer
Covestro Makroblend® UT305 PC/PET Blend
Covestro Makroblend® UT5205 PC/PBT Blend

PCOVEST0067 / 201850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.