MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makroblend® UT6007 PC+PBT
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: PC+PBT)-blend, impact modified, easy release, UV-stabilized, injection molding grade. Makroblend® UT6007 offers an exceptional low-temperature impact strength, good flowability and excellent chemical resistance.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inPost-shrinkage, 1 hr; 90°C; b.o. ISO 2577
 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in600 bar; b.o. ISO 2577
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
18 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 108 MPa15700 psiISO 2039-1
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.20 GPa319 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 80.0 MPa11600 psi2 mm/min; ISO 178
Flexural Yield Strength 70.0 MPa
@Strain 3.5 %
10200 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.15 GPa312 ksi2 mm/min; ISO 178
Flexural Strain at Yield 6.0 %6.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  20.0 kJ/m²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 180-A
 35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 45.0 kJ/m²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-U
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
Impact  3800
@Temperature 23.0 °C
3800
@Temperature 73.4 °F
[N], Puncture Max Force; ISO 6603-2
 5000
@Temperature -30.0 °C
5000
@Temperature -22.0 °F
[N], Puncture Max Force; ISO 6603-2
Puncture Energy  47.0 J
@Temperature 23.0 °C
34.7 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 58.0 J
@Temperature -30.0 °C
42.8 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.0045
@Frequency 1e+6 Hz
0.0045
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VSolution B, M; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FISO 75-1,-2
Vicat Softening Point 126 °C
@Load 5.10 kg
259 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index 21 %21 %Method A; ISO 4589-2
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FISO 294
Mold Temperature 70.0 °C158 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT3907 PC+PBT
Covestro Makroblend® AR205 PC+PET
Covestro Makroblend® UT6005 PC+PBT
Covestro Makrolon® 2807 Polycarbonate, Injection Grade
Covestro Makroblend® UT5207 PC/PBT Blend

PCOVEST0804 / 202587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.