MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Surlyn® PC350 Ionomer Resin, Highest Clarity, Sodium
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for processing by injection molding. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.

Data provided by the manufacturer.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Ultimate 22.0 MPa3190 psiASTM D638
Tensile Strength, Yield 16.0 MPa2320 psi50 mm/min cross speed; ASTM D638
Elongation at Break 325 %325 %ASTM D638
Flexural Modulus 0.448 GPa65.0 ksiASTM D790
Abrasion 360360NBS Index; ASTM D1630
 
Thermal PropertiesMetricEnglishComments
Melting Point 88.0 °C190 °FDSC
Vicat Softening Point 71.0 °C160 °FRate B, ASTM D1525-70
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 6.35 mm
5.0 %
@Thickness 0.250 in
ASTM D1003A
Gloss 143 %143 %20° per ASTM D523-6
Transmission, Visible 90 %90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium

PDU425 / 33076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.