MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 4047 Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Oil quenched. Forging temp.: 1230°C (2250°F) max. Annealing temp.: 790 - 845°C. Hardening temp.: 815 - 855°C. Tempered to desired hardness.

Applications: Used for small parts in severe conditions or non-critical larger parts that take advantage of the higher strength-to-weight ratio of alloy steel. A typical application would be parts in the steering assembly of an automobile.

Forms: billets, blooms, slabs, hot rolled bars, and cold finished bars.

Key Words: alloy steels, UNS G40470, ASTM A322, ASTM A331, ASTM A519, SAE J404 SAE J412, SAE J770
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 179 - 229179 - 229
Hardness, Knoop 226226Converted from Brinell
Hardness, Rockwell B 9393Converted from Brinell
Hardness, Rockwell C 1414Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 214214Converted from Brinell
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Calculated
Machinability 65 %65 %annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000245 ohm-cm0.0000245 ohm-cmTypical 4000 series steel
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical 4000 series steel
Thermal Conductivity 44.5 W/m-K309 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.45 - 0.50 %0.45 - 0.50 %
Iron, Fe 97.87 - 98.51 %97.87 - 98.51 %As remainder
Manganese, Mn 0.70 - 0.90 %0.70 - 0.90 %
Molybdenum, Mo 0.20 - 0.30 %0.20 - 0.30 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
AISI 4028 Steel
AISI 4012 Steel
AISI 4037 Steel
AISI 4063 Steel (UNS G40630)

M4047A / 7459

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.