MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³dry; ISO 1183
Water Absorption 7.0 %7.0 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.2 %2.2 %beginning dry (23°C/50% R.H.); ISO 62
Viscosity Number 145 cm³/g1.45 dl/g
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/inASTM Data; MD
Melt Flow 70 g/10 min
@Load 5.00 kg,
Temperature 275 °C
70 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 85.0 MPa12300 psi5mm/min; ISO 527
Elongation at Break 10 %10 %5mm/min; ISO 527
Tensile Modulus 4.50 GPa653 ksi1mm/min; ISO 527
Flexural Strength 125 MPa18100 psiISO Data
Flexural Modulus 4.00 GPa580 ksiISO Data
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO Test
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²ISO 179
Charpy Impact, Notched 1.10 J/cm²5.24 ft-lb/in²ISO 179
Tensile Creep Modulus, 1000 hours 2500 MPa363000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.16
@Frequency 1e+6 Hz
0.16
@Frequency 1e+6 Hz
IEC 60250
 0.30
@Frequency 100 Hz
0.30
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10 K/min
 260 °C500 °FASTM Test
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
NSF YesYesNSF Std. 51
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
EMS-Grivory Grilon® TSG-15/4 PA666-GF15
BASF Ultramid® A3EG3 BK00564 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)

PBASF9216 / 84980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.