MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek MTEK 275 Cast UNS C95900 Aluminum Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Engineered alloy for excellent wear and anti-galling properties in forming, bending and drawing dies. Aluminum Bronze heat treated to higher mechanical properties where necessary.

Information provided by MetalTek

Cast UNS C95900; Cast Grade C95900; Cast ASTM B271, B505, B148

Key Words: UNS C95900
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 248>= 2483000 kg
 2552553000 kg, typical
Tensile Strength, Ultimate >= 515 MPa>= 74700 psi
Tensile Strength, Yield >= 345 MPa>= 50000 psi
Elongation at Break >= 1.0 %>= 1.0 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 13 %13 %
Copper, Cu 82.5 %82.5 %
Iron, Fe 4.5 %4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCO® 22 Aluminum Bronze, Extruded Bar
Overview of materials for Silicone Rubber
Ampco Metal AMPCO® 21 Aluminum Bronze, Round, ≤ 50.8 mm.
MetalTek MTEK 175 Cast UNS C95400 Aluminum Bronze
Materion BrushBronze® 95510 (AMS 4880) Continuous Cast 0.250" - 4.0"

NMETEK009 / 18259

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.