MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® TP 202-027 901510 Nylon 66 (PA66), 30% Glass/Carbon Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: PA 66, 30% glass fibers/carbon fibers, injection molding, improved flowability, heat-aging stabilized, improved electrical conductivity

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.306 g/cc0.04718 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0028 cm/cm0.0028 in/in60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0077 cm/cm0.0077 in/in60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  700 N
@Temperature -30.0 °C
157 lb (f)
@Temperature -22.0 °F
ISO 6603-2
 840 N
@Temperature 23.0 °C
189 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Tensile Strength at Break 170 MPa24700 psi5 mm/min; ISO 527-1,-2
Elongation at Break 2.6 %2.6 %5 mm/min; ISO 527-1,-2
Tensile Modulus 11.8 GPa1710 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 255 MPa37000 psi2 mm/min; ISO 178-A
Flexural Modulus 11.4 GPa1650 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 2.9 %2.9 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  55.0 kJ/m²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 55.0 kJ/m²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
Puncture Energy  2.30 J
@Temperature -30.0 °C
1.70 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 3.10 J
@Temperature 23.0 °C
2.29 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmIEC 60093
Surface Resistance 10000 ohm10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point 261 °C502 °F10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) >= 250 °C>= 482 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-1,-2
Shrinkage, MD 0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
Shrinkage, TD 0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °Finjection molding
 280 - 300 °C536 - 572 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled
Envalior Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber
Celanese SO.F.TER Nylfor A® A2 GFCF/30 Nylon 66
Grupo Repol Dinalon® A1S25 G30 PA66 30% Glass Fiber
Lehvoss LUVOCOM® 1-0889-2 Polyamide 66 with carbon fiber and glass fiber, heat stabilized

PLANW9496 / 208376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.