MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Description & Application: PBHT-15 Plus is a rigid, High Density Urethane, (HDU), Tooling/Modeling board designed for Prototype Machining, Water Jet cutting, Pattern Making, Thermoforming, Prepreg Composite Layup Tooling, Vacuum Form Tooling, Tool Path Proofing, Lost Wax Casting Masters, Master Model Making, Artistic Carving Blocks, Indoor and Outdoor Signage. PBHT Plus is made in the USA.

Information provided by Costal Enterprises Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.240 g/cc0.00868 lb/in³ASTM D1623
Water Absorption 0.010 %
@Time 346000 sec
0.010 %
@Time 96.0 hour
by Volume; ASTM D2842
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ASTM D2240
Tensile Strength 2.80 MPa406 psiASTM D1623
Elongation at Break 5.3 %5.3 %
Tensile Modulus 0.2215 GPa32.12 ksiASTM D1623
Flexural Strength 3.49 MPa506 psiMethod 1A; ASTM D790
Flexural Modulus 0.11208 GPa16.256 ksiMethod 1A; ASTM D790
Compressive Strength 3.93 MPa570 psiASTM D1621
Compressive Modulus 0.14124 GPa20.485 ksiASTM D1621
Shear Modulus 0.02686 GPa3.895 ksiASTM C273
Shear Strength 2.59 MPa375 psiASTM C273
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 1.31.3ASTM D1678
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°F
Specific Heat Capacity 0.983 J/g-°C0.235 BTU/lb-°FASTM E1269
Maximum Service Temperature, Air 149 °C300 °FDry
Glass Transition Temp, Tg 140 °C284 °FDMA/TMA
 
Descriptive Properties
"K" Value Insulation Factor0.771ASTM C177
Closed Cell Content97%ASTM D2856
Dimensional Stability<1.2%ASTM D2126

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
RTP Company RTP 1200-70A  Polyurethane Thermoplastic Elastomer (TPU) 70 Shore A
Covestro Baydur® 40 Polyurethane
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,

PCOAS003 / 187036

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.