MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: 3 hrs @ 480-495°C or Mill Hardened

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: RWMA Class 3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 680 - 900 MPa98600 - 131000 psi
Tensile Strength, Yield 550 - 760 MPa79800 - 110000 psi
Elongation at Break >= 10 %>= 10 %
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 - 0.00000380 ohm-cm0.00000290 - 0.00000380 ohm-cm45-60% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 240 W/m-K1670 BTU-in/hr-ft²-°F
Melting Point 1040 - 1080 °C1900 - 1980 °F
Solidus 1040 °C1900 °F
Liquidus 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.20 - 0.60 %0.20 - 0.60 %
Copper, Cu 98 %98 %as balance
Nickel, Ni 1.4 - 2.2 %1.4 - 2.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy M25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Chromium-Copper, UNS C17600, TF00 Temper rod, bar, wire, tubing, plate, forged products
Materion Brush® 1916 Machinable Copper Nickel Alloy Wire, Temper HT (UNS C19160)
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375"
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200)

NBB690 / 15283

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.