MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shandong Dawn Dawnprene 624-80A TPV (EPDM/PP)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Uses: industrial castors

Information provided by Shandong Dawn Polymer Material Co.,Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.975 g/cc0.0352 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8383ISO 7619
Tensile Strength 9.85 MPa1430 psiISO 37
Elongation at Break 615 %615 %ISO 37
Compression Set 51 %
@Temperature 70.0 °C,
Time 79200 sec
51 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Descriptive Properties
Elongation Change (%) ISO 188-17.4change @ heat aging 100°C, 1000hr
Tensile Change (%) ISO 188-13.8change @ heat aging 100°C, 1000hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shandong Dawn Dawnprene 11-80A TPV (EPDM/PP)
Shandong Dawn Dawnprene 11-87av TPV (EPDM/PP)
Shandong Dawn Dawnprene 34-85A TPV (EPDM/PP)
Shandong Dawn Dawnprene 612-85A TPV (EPDM/PP)
Shandong Dawn Dawnprene 712-80A TPV (EPDM/PP)

PSHAND974 / 192610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.