MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hifax RTA3223 WA6247 GRY Thermoplastic Olefinic Elastomer (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax RTA3223 WA6247 GRY medium melt flow, 1,600 MPa flexural modulus, paintable, mineral filled thermoplastic olefin (TPO) resin has a very good combination of strength, stiffness and dimensional stability. It is typically used for rigid automotive exterior ornamentation applications. Typical applications include automotive claddings and rocker panels, license plate brackets, appliques, filler panels and grilles. Applications: Automotive Parts, Exterior Automotive Applications.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Yield 18.0 MPa2610 psiASTM D 638
Elongation at Break 50 %50 %ASTM D638
Flexural Modulus 1.60 GPa232 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature -30.0 - 100 °C
27.8 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D 696
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elastocon TPE Technologies Elastocon® SMR1600 Thermoplastic Polyolefin Elastomer
Avient Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE))
Avient Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
LyondellBasell Hifax TRC 835X BLK Thermoplastic Olefinic Elastomer
LyondellBasell Hifax TRC 779P 578Q LT SILVER MET Thermoplastic Olefinic Elastomer (TPO)

PEQT7280 / 218917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.