MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Flex® TPE A 4002 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Multi-Flex® A 4002 is based on Shell's Kraton G polymer and is suitable for soft touch applications for the automotive industry. It exhibits excellent paintibility adhesion. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Flow 4.0 g/10 min4.0 g/10 min(Condition L) ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 545410 sec; ASTM D-2240
Tensile Strength, Ultimate 4.80 MPa696 psiASTM D412
Elongation at Break 1400 %1400 %ASTM D412
Flexural Modulus 0.0117 GPa1.70 ksimethod 1, Proc.B; ASTM D-790
Tear Strength 26.6 kN/m152 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flex® TPE A 7007 BLK
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Multibase Multi-Flex® TPE A 6006 BLK
Kuraray HYBRAR® Blends
Multibase Multi-Flex® TPE A 6421 BLK

PLA005 / 49466

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.