MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Novaduran® 5820G40H Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled

Material Notes: Low warpage high strength. 40% GF Reinforced alloy UL-HB grade. Excellent mechanical properties. Excellent heat resistance. Excellent moldability and flowability. Low moisture absorption rate for high dimensional stability. Excellent surface gloss and color. Excellent oil and chemical resistance. Excellent electrical properties. Excellent friction and abrasion resistance. Flame retardant grades also available.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Water Absorption 0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
Immersion
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
0.0030 in/in
@Thickness 0.0787 in
100 mm long x 100 mm wide
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
0.0090 in/in
@Thickness 0.0787 in
100 mm long x 100 mm wide
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psiISO 527-1,2
Elongation at Break 2.0 %2.0 %ISO 527-1,2
Tensile Modulus 12.5 GPa1810 ksiISO 527-1,2
Flexural Strength 240 MPa34800 psiISO 178
Flexural Modulus 11.5 GPa1670 ksiISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+16 ohm-cm6.00e+16 ohm-cmIEC 60093
Surface Resistance 9.00e+15 ohm9.00e+15 ohmIEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength  26.0 kV/mm
@Thickness 2.00 mm
660 kV/in
@Thickness 0.0787 in
IEC 60243-1
 32.0 kV/mm
@Thickness 1.00 mm
813 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  10.0 µm/m-°C
@Temperature -30.0 - 120 °C
5.56 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359-2
 10.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
5.56 µin/in-°F
@Temperature -22.0 - 122 °F
ISO 11359-2
 10.0 µm/m-°C
@Temperature 50.0 - 120 °C
5.56 µin/in-°F
@Temperature 122 - 248 °F
ISO 11359-2
CTE, linear, Transverse to Flow  70.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
38.9 µin/in-°F
@Temperature -22.0 - 122 °F
ISO 11359-2
 100 µm/m-°C
@Temperature -30.0 - 120 °C
55.6 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359-2
 130 µm/m-°C
@Temperature 50.0 - 120 °C
72.2 µin/in-°F
@Temperature 122 - 248 °F
ISO 11359-2
Melting Point 224 °C435 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) <= 220 °C<= 428 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Novaduran® 5010CTN33 Polybutylene Terephthalate
Mitsubishi Novaduran® 5810G40 Polybutylene Terephthalate
Mitsubishi Novaduran® 5710F40 Polybutylene Terephthalate
Mitsubishi Novaduran® 5010GPN33 Polybutylene Terephthalate
Mitsubishi Novaduran® 5010G45 Polybutylene Terephthalate

PMITSU9070 / 191743

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.