MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Flexirene® MR 50 U Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.

Parts made with Flexirene MR 50 U are characterized by optimum rigidity.Main Applications: Flexirene MR 50 U is recommended for the production of thin walled containers requiring high mechanical properties, lids, caps, closures, houseware and shock absorbers.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.939 g/cc0.939 g/ccISO 1183
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
22 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ISO 868/A
Tensile Strength at Break 15.0 MPa2180 psiISO 527
Tensile Strength, Yield 15.0 MPa2180 psiISO 527
Elongation at Break >= 500 %>= 500 %ISO 527
Flexural Modulus 0.500 GPa72.5 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °FInternal method
Vicat Softening Point 112 °C
@Load 1.00 kg
234 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® FB2310 LLDPE for Film
Braskem LL6802N LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem LL6801N LLDPE Blown Film Extrusion Polyethylene Copolymer
Braskem LF320 LLDPE Cast Film Extrusion Polyethylene Copolymer
Braskem LF0720/20AF Blown Film Extrusion Linear Low Density Polyethylene

PENG100 / 124494

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.