MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Casico™ FR6083 Reduced Fire Hazard Jacketing Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Casico™ FR6083 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural jacketing compound combining with excellent extrusion properties. The composition is based on the elements Carbon, Hydrogen, Oxygen, Silicon and Calcium. Compounds based on these elements will therefore be the only significant constituents of the combustion fumes. Other elements may be present in concentrations less than 0.1%. Applications: jacket for energy cables. The principal feature of this compound is the high physical strength and toughness. It can be used in areas sensitive to smoke or corrosive and toxic combustion products. For most cable constructions, Casico™ FR6083 has sufficient flame retardancy to satisfy single wire vertical burning tests. Specifications: HD 603 S1; EN 50363-8; IEC 60840, Type ST7; IEC 60502, Type ST7; and IEC 60502, Type ST8

Information provided by Borealis AG

Key Words: PE; Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1872-2/ISO 1183
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 535315s; ISO 868
Tensile Strength at Break 2.25 MPa326 psiafter aging, 240h, 100°C; or UV aging; IEC 60811-1-2
 15.0 MPa2180 psi50mm/min; IEC 60811-1-1
Elongation at Break 75 %75 %after aging, 7h, 110°C; IEC 60811-1-2
 500 %500 %IEC 60811-1-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.80e+6 ohm-cm1.80e+6 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 28 %28 %ISO 4589A
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 170 °C338 °F
Zone 3 180 °C356 °F
Zone 4 190 °C374 °F
Die Temperature 190 °C374 °F
 
Descriptive Properties
High Temperature Pressure Test, %15110°C, 6h; IEC 60811-3-1
 5105°C, 6h; IEC 60811-3-1
Single Vertical Flame TestPassIEC 602431

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
AlphaGary Megolon™ S380 Low Smoke Halogen Free
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables
AlphaGary Smokeguard™ O 303 Low Smoke Halogen Free
AlphaGary Smokeguard™ O 204 Low Smoke Halogen Free

PBOREA402 / 108661

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.