MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Indium Alloy
Categories: Metal; Nonferrous Metal; Indium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Indium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.27 - 9.33 g/cc0.263 - 0.337 lb/in³Average value: 7.72 g/cc Grade Count:59
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 0.900 - 11.00.900 - 11.0Average value: 5.09 Grade Count:12
Tensile Strength, Ultimate 1.90 - 164 MPa276 - 23800 psiAverage value: 25.2 MPa Grade Count:36
Elongation at Break 22.0 - 83.0 %22.0 - 83.0 %Average value: 61.9 % Grade Count:6
Shear Strength 6.10 - 18.5 MPa885 - 2680 psiAverage value: 12.4 MPa Grade Count:7
Adhesive Bond Strength 6.00 - 18.5 MPa870 - 2680 psiAverage value: 12.4 MPa Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000720 - 0.0000520 ohm-cm0.00000720 - 0.0000520 ohm-cmAverage value: 0.0000220 ohm-cm Grade Count:27
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 33.0 µm/m-°C8.33 - 18.3 µin/in-°FAverage value: 25.0 µm/m-°C Grade Count:26
Thermal Conductivity 22.0 - 82.0 W/m-K153 - 569 BTU-in/hr-ft²-°FAverage value: 45.9 W/m-K Grade Count:7
Melting Point 60.0 - 237 °C140 - 459 °FAverage value: 142 °C Grade Count:59
Solidus 60.0 - 184 °C140 - 363 °FAverage value: 136 °C Grade Count:51
Liquidus 60.0 - 237 °C140 - 459 °FAverage value: 147 °C Grade Count:51
Boiling Point 2000 - 2080 °C3630 - 3780 °FAverage value: 2060 °C Grade Count:4
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 15.0 - 50.0 %15.0 - 50.0 %Average value: 34.7 % Grade Count:3
Bismuth, Bi 0.0000100 - 33.7 %0.0000100 - 33.7 %Average value: 15.6 % Grade Count:11
Cadmium, Cd 0.0000100 - 26.0 %0.0000100 - 26.0 %Average value: 9.83 % Grade Count:10
Copper, Cu 0.00000500 - 0.00420 %0.00000500 - 0.00420 %Average value: 0.000757 % Grade Count:6
Gallium, Ga 0.400 - 0.700 %0.400 - 0.700 %Average value: 0.550 % Grade Count:4
Indium, In 44.0 - 100 %44.0 - 100 %Average value: 75.2 % Grade Count:63
Iron, Fe 0.0000150 - 0.000300 %0.0000150 - 0.000300 %Average value: 0.0000858 % Grade Count:6
Lead, Pb 0.0000180 - 50.0 %0.0000180 - 50.0 %Average value: 22.1 % Grade Count:23
Nickel, Ni 0.0000190 - 0.000500 %0.0000190 - 0.000500 %Average value: 0.000270 % Grade Count:4
Silver, Ag 0.000100 - 10.0 %0.000100 - 10.0 %Average value: 4.50 % Grade Count:14
Thallium, Tl 0.00000900 - 0.000200 %0.00000900 - 0.000200 %Average value: 0.0000563 % Grade Count:6
Tin, Sn 0.0000100 - 52.0 %0.0000100 - 52.0 %Average value: 26.6 % Grade Count:23
Trace Metals 0.0000200 - 0.0000320 %0.0000200 - 0.0000320 %Average value: 0.0000240 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
In90-Ag10 Indium-Silver Solder
In97-3Ag Indium-Silver Solder
Indium Corp. 3N Commercial Indium Metal
AIM 97In/3Ag Solder for Photonic Packaging
Indium, In

M01057 / 81670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.