MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 30%Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.46 - 1.70 g/cc0.0527 - 0.0614 lb/in³Average value: 1.60 g/cc Grade Count:20
Filler Content 25.0 - 30.0 %25.0 - 30.0 %Average value: 29.5 % Grade Count:10
Water Absorption 0.300 - 1.60 %0.300 - 1.60 %Average value: 0.446 % Grade Count:13
Additive Loading 30.0 %30.0 %Average value: 30.0 % Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.00500 cm/cm0.00100 - 0.00500 in/inAverage value: 0.00226 cm/cm Grade Count:19
Linear Mold Shrinkage, Transverse 0.00580 - 0.00800 cm/cm0.00580 - 0.00800 in/inAverage value: 0.00660 cm/cm Grade Count:3
Melt Flow 4.50 - 25.0 g/10 min4.50 - 25.0 g/10 minAverage value: 14.7 g/10 min Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120 - 123120 - 123Average value: 123 Grade Count:7
Tensile Strength, Ultimate 60.0 - 150 MPa8700 - 21800 psiAverage value: 130 MPa Grade Count:16
 10.0 - 135 MPa
@Temperature 60.0 - 150 °C
1450 - 19600 psi
@Temperature 140 - 302 °F
Average value: 100 MPa Grade Count:2
Tensile Strength, Yield 125 - 169 MPa18200 - 24500 psiAverage value: 142 MPa Grade Count:5
Elongation at Break 1.40 - 4.00 %1.40 - 4.00 %Average value: 2.42 % Grade Count:19
 2.10 - 2.50 %
@Temperature 60.0 - 150 °C
2.10 - 2.50 %
@Temperature 140 - 302 °F
Average value: 2.33 % Grade Count:1
Modulus of Elasticity 6.60 - 10.9 GPa957 - 1580 ksiAverage value: 9.38 GPa Grade Count:18
 8.60 - 10.0 GPa
@Temperature 60.0 - 160 °C
1250 - 1450 ksi
@Temperature 140 - 320 °F
Average value: 9.41 GPa Grade Count:2
Flexural Yield Strength 172 - 221 MPa25000 - 32100 psiAverage value: 193 MPa Grade Count:17
Flexural Modulus 7.58 - 11.3 GPa1100 - 1640 ksiAverage value: 8.54 GPa Grade Count:17
Compressive Yield Strength 124 - 145 MPa18000 - 21000 psiAverage value: 140 MPa Grade Count:5
Fatigue Strength  31.0 - 43.0 MPa
@# of Cycles 100000 - 1.00e+7
4500 - 6240 psi
@# of Cycles 100000 - 1.00e+7
Average value: 37.3 MPa Grade Count:1
 31.0 - 43.0 MPa
@Temperature 180 - 180 °C
4500 - 6240 psi
@Temperature 356 - 356 °F
Average value: 37.3 MPa Grade Count:1
Shear Modulus 0.200 - 1.00 GPa
@Temperature 50.0 - 225 °C
29.0 - 145 ksi
@Temperature 122 - 437 °F
Average value: 0.762 GPa Grade Count:1
Izod Impact, Notched 0.641 - 1.07 J/cm1.20 - 2.00 ft-lb/inAverage value: 0.831 J/cm Grade Count:16
Izod Impact, Unnotched 3.74 - 7.47 J/cm7.00 - 14.0 ft-lb/inAverage value: 5.91 J/cm Grade Count:13
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 42.0 - 59.0 kJ/m²
@Temperature -25.0 - 120 °C
20.0 - 28.1 ft-lb/in²
@Temperature -13.0 - 248 °F
Average value: 52.7 kJ/m² Grade Count:1
Charpy Impact Unnotched 2.50 - 4.20 J/cm²11.9 - 20.0 ft-lb/in²Average value: 3.40 J/cm² Grade Count:3
 4.50 - 4.50 J/cm²
@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.600 - 0.800 J/cm²2.86 - 3.81 ft-lb/in²Average value: 0.733 J/cm² Grade Count:3
 0.800 - 0.800 J/cm²
@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.800 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 2.00e+16 ohm-cm1.00e+12 - 2.00e+16 ohm-cmAverage value: 7.69e+15 ohm-cm Grade Count:13
Surface Resistance 1.00e+14 - 1.00e+15 ohm1.00e+14 - 1.00e+15 ohmAverage value: 4.00e+14 ohm Grade Count:3
Dielectric Constant 4.11 - 4.304.11 - 4.30Average value: 4.20 Grade Count:6
Dielectric Strength 14.6 - 37.0 kV/mm370 - 940 kV/inAverage value: 18.7 kV/mm Grade Count:9
Dissipation Factor 0.00180 - 0.01000.00180 - 0.0100Average value: 0.00590 Grade Count:6
Arc Resistance 75.0 - 120 sec75.0 - 120 secAverage value: 84.0 sec Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 36.0 µm/m-°C8.33 - 20.0 µin/in-°FAverage value: 27.6 µm/m-°C Grade Count:10
 17.0 - 17.0 µm/m-°C
@Temperature 140 - 180 °C
9.44 - 9.44 µin/in-°F
@Temperature 284 - 356 °F
Average value: 17.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.230 - 0.317 W/m-K1.60 - 2.20 BTU-in/hr-ft²-°FAverage value: 0.295 W/m-K Grade Count:4
Maximum Service Temperature, Air 185 - 220 °C365 - 428 °FAverage value: 203 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 215 - 222 °C419 - 432 °FAverage value: 219 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 204 - 220 °C400 - 428 °FAverage value: 213 °C Grade Count:20
Glass Transition Temp, Tg 225 °C437 °FAverage value: 225 °C Grade Count:3
Flammability, UL94 V-0V-0Grade Count:16
Oxygen Index 40.0 - 44.5 %40.0 - 44.5 %Average value: 42.2 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 343 - 366 °C650 - 690 °FAverage value: 354 °C Grade Count:6
Melt Temperature 343 - 399 °C649 - 750 °FAverage value: 364 °C Grade Count:10
Mold Temperature 135 - 190 °C275 - 374 °FAverage value: 158 °C Grade Count:15
Drying Temperature 149 - 180 °C300 - 356 °FAverage value: 155 °C Grade Count:8
Moisture Content 0.0400 %0.0400 %Average value: 0.0400 % Grade Count:5
Dew Point -31.7 °C-25.0 °FAverage value: -31.7 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa10000 - 15000 psiAverage value: 86.2 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
Overview of materials for Polyethersulfone (PES)
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

O3713 / 78241

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.