MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter Invar 36® Alloy, Cold Drawn Bars
Categories: Metal; Electronic/Magnetic Alloy; Superalloy; Iron Base

Material Notes: Data provided by Carpenter Technology Corporation.

Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. This alloy has been used for applications where dimensional changes due to temperature variation must be minimized, such as in radio and electronic devices, aircraft controls, optical and laser systems, etc. This alloy has also been used in conjunction with high expansion alloys where a motion is desired when the temperature changes, such as in bimetallic thermostats and in rod and tube assemblies for temperature regulators.

Invar 36® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS K93601; ASTM B753 Alloy T36
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9090
Tensile Strength, Ultimate 621 MPa90100 psi
Tensile Strength, Yield 483 MPa
@Strain 0.2 %
70100 psi
@Strain 0.2 %
Elongation at Break 20 %20 %in 50.8 mm
Reduction of Area 60 %60 %
Modulus of Elasticity 148 GPa21500 ksi(Cold Rolled)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000820 ohm-cm0.0000820 ohm-cmTemperature Coefficient = 0.0011/K (21-100°C)
Curie Temperature 279 °C534 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  1.30 µm/m-°C
@Temperature 93.0 °C
0.722 µin/in-°F
@Temperature 199 °F
 4.18 µm/m-°C
@Temperature 260 °C
2.32 µin/in-°F
@Temperature 500 °F
 7.60 µm/m-°C
@Temperature 371 °C
4.22 µin/in-°F
@Temperature 700 °F
Specific Heat Capacity 0.515 J/g-°C0.123 BTU/lb-°F
Thermal Conductivity 10.15 W/m-K70.44 BTU-in/hr-ft²-°F
Melting Point 1427 °C2601 °F
Solidus 1427 °C2601 °FMelting Point
Liquidus 1427 °C2601 °FMelting Point
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %
Iron, Fe 63 %63 %as remainder
Manganese, Mn 0.35 %0.35 %
Nickel, Ni 36 %36 %
Silicon, Si 0.20 %0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Invar 36® Alloy, Annealed Bars and Strip
Carpenter Invar 36® Alloy, Cold Rolled Strip
Carpenter Super Invar 32-5
Aperam Invar® FeNi336 Cold Rolled Strip
Aperam Invar® Controlled Expansion Alloys Iron-Nickel Alloys

NCAR00 / 15582

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.