MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability, and impact strength over a wide temperature range. Recommended sterilization techniques for Radel R4400 include EtO gas, radiation, steam autoclaving, dry heat and cold sterilization.

Radel® is a trade name of Solvay Advanced Polymers. Information provided by Westlake Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Water Absorption 0.35 %0.35 %ASTM D570; 24 hrs.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 69.6 MPa10100 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Elongation at Yield 7.2 %7.2 %ASTM D638
Tensile Modulus 2.34 GPa340 ksiASTM D638
Flexural Yield Strength 97.2 MPa14100 psiASTM D790
Flexural Modulus 2.54 GPa368 ksiASTM D790
Compressive Yield Strength 97.97 MPa14210 psiASTM D695
Compressive Modulus 1.99 GPa288 ksiASTM D695
Izod Impact, Notched 2.67 J/cm5.00 ft-lb/inASTM D256; Depends on pigment
Izod Impact, Unnotched NBNBASTM D256
Tensile Impact Strength 367 kJ/m²175 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C
@Temperature 20.0 °C
31.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.349 W/m-K2.42 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.787 mm
V-0
@Thickness 0.0310 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
RTP Company RTP Radel R-7625 Polyphenyl Sulfone (PPSU); Flame Retardant
Westlake Plastics Propylux® HS Polypropylene-heat stabilized For Medical Applications
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized
Westlake Plastics Tempalux® Polyetherimide For Medical Applications

PWEST102 / 72748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.