MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODOLINE® OTE 500 Surfactant
Categories: Fluid

Material Notes: Description: Open time additive for zero to low VOC paints.

Identification: DEFOAMER BLEND

Available in: Asia Pacific, Europe, Latin America and North America.

Applications: RHODOLINE© OTE 500 is an APE-free and solvent-free additive and can be used for both resin and waterborne paint formulations to extend open time as well as improve film gloss, stain removal, and pigment dispersion. RHODOLINE© OTE 500 can be post added to the resin emulsion at usage levels of 1 to 6 % based on total weight. RHODOLINE© OTE 500 can also be formulated in waterborne paints at typically 0.5 to 3 % based on total formulation.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.026 - 1.226 g/cc0.03707 - 0.04429 lb/in³RP-17617
Solids Content 78 - 82 %78 - 82 %CEM 30% Power; RP-0528
pH 4.0 - 7.04.0 - 7.05% Solution; RP-0420
Viscosity <= 5000 cP<= 5000 cP#4 sp @ 60 rpm; RP-0596
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceClear to Hazy, Slightly Amber to Yellow LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODOLINE® DF 540 Surfactant
Solvay RHODOLINE® DF-988 Surfactant
Solvay RHODOLINE® WA-100 Surfactant
Solvay RHODAPEX® CD-128 Surfactant
Solvay RHODAPEX® AB 20 Surfactant

WRHOD491 / 137722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.