MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with excellent optics, good stiffness and strong heat sealing characters can be produced from these resins.

Regulatory Status: The NA426 resins meet the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "...in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for further information.

NA426 resins have excellent drawdown characteristics that yield outstanding output rates. Recommended extrusion conditions are 330°-380°F (166°-194°C) melt temperatures and a blow-up ratio between 1.7-3.0:1.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Vinyl Acetate Content 2.5 %2.5 %
Thickness 31.8 microns1.25 mil
Melt Flow 2.5 g/10 min2.5 g/10 minASTM D1238
Antiblock Level 1900 ppm1900 ppm
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 350 %350 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Elmendorf Tear Strength MD 220 g220 gASTM D1922
Elmendorf Tear Strength TD 250 g250 gASTM D1922
Dart Drop 2.52 g/micron64.0 g/milF50; ASTM D1709
Film Tensile Strength at Break, MD 22.8 MPa3300 psiASTM D882
Film Tensile Strength at Break, TD 16.5 MPa2400 psiASTM D882
1% Secant Modulus, MD 138 MPa20000 psiASTM E111
1% Secant Modulus, TD 172 MPa25000 psiASTM E111
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.5 %4.5 %ASTM D1003
Gloss 73 %73 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 °C375 °F
Die Opening 0.0635 cm0.0250 in
Blow-up Ratio (BUR) 2.02.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 30 EVA + PE Foam
Dow Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin
ExxonMobil LD 141.87 Shrink Film Resin
ExxonMobil LD 144.50 Packaging Film Resin
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer

PEQU0843 / 104199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.