MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® BMNO P40 TLD PA11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
 1.05 g/cc0.0379 lb/in³Cond.; ISO 1183
Water Absorption 1.6 %1.6 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/in
 0.012 cm/cm0.012 in/inDry; ISO 294-4, 2577
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 235 °C
35 g/10 min
@Load 4.76 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 58
@Time 15.0 sec
58
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength, Yield 25.0 MPa3630 psiCond.; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 42 %42 %Cond.; ISO 527-1/-2
Tensile Modulus 0.345 GPa50.0 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmCond.; IEC 60093
Surface Resistance 5.00e+11 ohm5.00e+11 ohmCond.; IEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 23.0 kV/mm584 kV/inCond.; IEC 60243-1
Dissipation Factor  0.0964
@Frequency 1e+6 Hz
0.0964
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.179
@Frequency 100 Hz
0.179
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FDry; ISO 11359-1/-2
Melting Point 181 °C358 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FDry; ISO 75-1/-2
Vicat Softening Point 140 °C284 °F50°C/h 50N; Dry; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 50.0 °C122 °FInjection Molding; ISO 10724
Hold Pressure 16.0 MPa2320 psiInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based88ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
PlasticizerYes
Processing MethodsInjection Molding
Release agentYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® BMNO P20 TLD PA11
Arkema Rilsan® BECNO TL PA11
Arkema Rilsan® BMNO PA11
Arkema Rilsan® BSR 30 PA11-CF30
Arkema Rilsan® BMNO TEX PA11

PARKF900 / 193640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.