MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and designed to be processed using especially adapted physical foam extrusion lines. Supplied as free-foaming pellets in 25 kilogram (55 pound) moisture barrier bags.

Features:

  • Fast, easy injection molding, especially for complex part geometries
  • Good Sealing Performance
  • Excellent surface aspect
  • Minimal part warpage
  • Can be injected at lower molding temperatures or at lower injection pressures
  • Low odor
  • Very low fogging

Product Notes: Values are for injection molded plaques, side gated.
82.6 mm x 117.5 mm x 3 mm

Information provided by Advanced Elastomer Systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73735 seconds; ASTM D2240
Tensile Strength at Break 8.48 MPa1230 psiAcross flow; ASTM D412
Tensile Stress at Strain 3.60 MPa
@Strain 100 %
522 psi
@Strain 100 %
across flow; ASTM D412
Elongation at Break 460 %460 %Across flow; ASTM D412
Tear Strength 13.0 kN/m74.0 pli212°F; ASTM D624
 28.0 kN/m160 pli73°F; ASTM D624
Compression Set  24 %
@Temperature 22.8 °C,
Time 612000 sec
24 %
@Temperature 73.0 °F,
Time 170 hour
ASTM D395
 38 %
@Temperature 100 °C,
Time 612000 sec
38 %
@Temperature 212 °F,
Time 170 hour
ASTM D395
Tensile Set 14 %14 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °FContinuously for 1000 hours
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Drying Temperature 82.0 °C180 °FDesiccant Dryer
Dry Time 3 hour3 hourDesiccant Dryer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-80M300 Thermoplastic Rubber
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer

PADW154 / 22872

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.