MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials SILTEX® 18 Amorphous Silica Textile
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Material Notes: Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use where severe temperature conditions exist.

SILTEX 18 is manufactured to a finished weight of 18 ounces per square yard. Its unique properties make it well suited for protection of personnel and equipment against moderate welding splatter sparks, grinding of metals, etc. SILTEX 18 is also excellent for use in engineered thermal insulation systems designed for severe temperatures, such as Turbine Covers, Exhaust Silencer Covers, etc.

The amorphous silica fibers that make up all SILTEX products are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium.

All SILTEX fabrics are available in standard “C” and pre-shrunk (fired) versions; Fabrics are available with several coating/treatment options that enhance certain properties of the product in order to meet required performance characteristics.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.8286 g/cc0.02993 lb/in³Calculated from weight of 18 oz/sy
Thickness 737 microns29.0 milnom
 
Thermal PropertiesMetricEnglishComments
Melting Point 1700 °C3100 °F
Maximum Service Temperature, Air 982 °C1800 °FContinuous
 1260 °C2300 °FIntermittent use
Shrinkage 8.0 - 12 %
@Temperature 982 °C
8.0 - 12 %
@Temperature 1800 °F
Linear
 <= 3.0 %
@Temperature 704 °C,
Time 1800 sec
<= 3.0 %
@Temperature 1300 °F,
Time 0.500 hour
Linear
 
Descriptive Properties
Break StrengthMin 200 x 150 lbnom, warp x fill (1" x 4")
ConstructionWoven fabric, 8 harness satin weave
MaterialAmorphous Silica 96-99%
Packaging50 ly per roll or 300 ly master roll
Tolerance10%
Width, standard36 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile
Crystex Composites Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Thermal Ceramics K-Shield Felt AG/Min-K Composite
E-Glass Fiber, Generic
Microtherm Group Hydrophoblic Quilted Panel Filament Reinforced Silica Thermal Insulation Panel, Flexible and Waterproof

CMID04 / 1508

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.