MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow Hot Pressed Silicon Nitride Si3N4
Categories: Ceramic; Nitride

Material Notes: Hot pressing of Silicon Nitride produces a material of virtually zero porosity. This hard, grey ceramic is still very lightweight. Silicon Nitride shows good resistance to wear and abrasion. It shows very little oxidation at elevated temperatures, and high hardness and strength above 1000°C. One of its main assets is its resistance to thermal shock, due to the low thermal expansion coefficient. This material can be diamond ground to precise tolerances. It is used in gas turbine situations, as diesel engine components and as a electrical insulators.

Information provided by Goodfellow.

Key Words: Si3N4; HPSN; NITRASIL® R
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.11 g/cc0.112 lb/in³
Porosity 0.00 %0.00 %Apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 1700 - 22001700 - 2200kgf/mm²
Tensile Modulus 280 - 310 GPa40600 - 45000 ksi
Compressive Strength 2000 - 3500 MPa290000 - 508000 psi
Shear Strength 480 - 960 MPa69600 - 139000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 - 1.00e+15 ohm-cm1.00e+12 - 1.00e+15 ohm-cm
Dielectric Constant 1010
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.30 µm/m-°C
@Temperature 20.0 - 1000 °C
1.83 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.680 - 0.800 J/g-°C0.163 - 0.191 BTU/lb-°F
Thermal Conductivity 15.0 - 43.0 W/m-K104 - 298 BTU-in/hr-ft²-°F
Sublimation Temperature 1900 °C3450 °F
Maximum Service Temperature, Inert 1650 °C3000 °F
 
Component Elements PropertiesMetricEnglishComments
Si3N4 100 %100 %
 
Descriptive Properties
Chemical Resistance - AlkalisGood - Poor
Chemical Resistance - Concentrated AcidsFair
Chemical Resistance - Dilute AcidsGood
Chemical Resistance - HalogensGood - Poor
Chemical Resistance - MetalsFair

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Silicon Nitride, reaction sintered
Silicon Nitride, Si3N4
Goodfellow Gas Pressure Sintered Silicon Nitride Si3N4
Fused Quartz

CGOODF247 / 197410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.