MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite PYROGRAPH Ion Implant Grade Graphite
Categories: Carbon; Graphite

Material Notes: Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process seals the graphite surface and reduces particle generation in the chamber.
The manufacturing process begins with a specially formulated graphite. Once a part has been machined, it goes through a purification process that typically results in a purity level of < 2ppm. The final step is a pyrolytic vapor infiltration that produces a hard, uniform surface. Vapor phase processing allows deeper penetration of the pyrolytic carbon into the base material.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.56 g/cc0.0564 lb/in³
Particle Size 5.0 µm5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666
Flexural Strength 53.4 MPa7750 psi
Compressive Strength 97.9 MPa14200 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00201 ohm-cm0.00201 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.50 µm/m-°C4.17 µin/in-°F
 
Descriptive Properties
Purity99.9995 percent
Pyrolytic Carbon12% pick-up

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carlisle 201LL Carbon-Carbon Composite
Momentive Performance Materials "PG" Pyrolytic Graphite
LTI Carbon with Silicon Carbon used in heart valve prostheses
LTI Carbon used in heart valve prostheses
Momentive Performance Materials HTR1002 PBN/PG Heating Element

CPOCO24 / 85601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.