MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2V-3X V0 is halogen free and free of red phosphorous. RoHS: Grivory HT2V-3X V0 is in compliance with RoHS (2002/95/EC, Restriction of Hazardous Substances) WEEE: Parts produced from Grivory HT2V-3X V0 are not subject to "selective treatment" according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. ISO polymer designation: PA 6T/66 ASTM-designation: PPA, polyphthalamide. The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT2V-3X V0 is especially suitable for injection molded parts in electrical and electronic applications with high requirements and a material flame class acc. UL 94 V-0. The Material is suitable for lead-free SMT reflow soldering acc. e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL2 are achievable.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Water Absorption 3.5 %3.5 %ISO 62
Moisture Absorption 1.30 %1.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 230 MPa33400 psiconditioned; ISO 2039-1
 240 MPa34800 psidry; ISO 2039-1
Tensile Strength at Break 130 MPa18900 psiconditioned; ISO 527-1/-2
 140 MPa20300 psidry; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %dry; ISO 527-1/-2
 2.0 %2.0 %conditioned; ISO 527-1/-2
Tensile Modulus 10.5 GPa1520 ksiconditioned; ISO 527-1/-2
 10.5 GPa1520 ksidry; ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²dry; ISO 179/1eU
 4.00 J/cm²19.0 ft-lb/in²conditioned; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²dry; ISO 179/1eA
 0.700 J/cm²3.33 ft-lb/in²conditioned; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmdry; IEC 60093
 1.00e+12 ohm-cm1.00e+12 ohm-cmconditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 34.0 kV/mm864 kV/indry; IEC 60243-1
 34.0 kV/mm864 kV/inconditioned; IEC 60243-1
Comparative Tracking Index 600 V600 Vconditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C25.0 µin/in-°FISO 11359-1/-2
Melting Point 310 °C590 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C302 °Flong term; EMS
 240 °C464 °Fshort term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 190 °C374 °FISO 75-1/-2
Flammability, UL94 V-0V-0IEC 60695-11-10
 5VA5VAIEC 60695-11-20
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 35 %35 %ISO 4589-1/-2
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Interior
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
 Lighting
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
ProcessingInjection Molding
Product AttributesCo Polyamide
 Improved alcohol resistance
 Improved flowability and demolding
 Partially aromatic Polyamide
Special CharacteristicsFlame retardant
 Improved heat resistance

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese VECTRA C130 LCP, 30% Glass Reinforced
Celanese Thermx® CG933 NC010 PCT
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35

PGRH386 / 157095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.