MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui UNISTOLE™ R-100K Polyolefinic Primer/ Adhesive
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: UNISTOLE™ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent.

Characteristics
  • Excellent adhesion to various metals
  • Exceptional heat resistance and heat resistant adhesion
  • Good resistance to retort treatment
  • Useable with simple equipment such as gravure coaters, roll coaters and sprays
  • UNISTOLE™ R contains no chlorine

Applications
  • Adhesive for bonding metal foil and a polyolefin such as aluminum foil and PP film to make retort packages, PTP packages, easy peal packages, etc.
  • Metal coating agent (bonding of metal by extruding PP onto it, automotive parts, etc.)
  • Modifier when added to paints, adhesives, printing inks, since it improves adhesion to PP

Information provided by Mitsui Chemicals America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 10 µm10 µmAverage Particle Diameter
Viscosity 10 cP10 cPB-type viscometer (60rpm)
Viscosity Measurement 8.08.0[sec]; Zahn Cup
Collected Volatile Condensable Material 80 %80 %
 
Descriptive Properties
RemarksStandard Type

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® VaporCoat® 2200R MVTR
Mitsui UNISTOLE™ P-801 Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-902M Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-902 Polyolefinic Primer/ Adhesive
Mitsui UNISTOLE™ P-401A Polyolefinic Primer/ Adhesive

PMIT132 / 53290

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.