MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen ACP 9240 PLUS High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Hostalen ACP 9240 Plus is a high density polyethylene characterized by superior toughness and stiffness. Hostalen ACP 9240 Plus can be converted on HDPE blown film equipment with a homogeneous appearance and very low gel level. The very good bubble stability permits the production of wrinkle free and flat films within a wide range of blow up ratios. Typical applications are carrier and meat bags, inliners for drums, paper bags and FIBC as well as heavy duty bags. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Heavy Duty Packaging, Industrial Packaging, Lamination Film, Liner Film, Products for Use in Property Modification

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ISO 1183-1
Melt Flow  0.20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.20 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiISO 527-1,-2
Film Elongation at Break, MD 350 %350 %ISO 527-1,-3
Film Elongation at Break, TD 400 %400 %ISO 527-1,-3
Tensile Modulus 0.900 GPa131 ksiISO 527-1,-2
Dart Drop Test >= 300 g>= 0.662 lb
Film Tensile Strength at Break, MD 80.0 MPa11600 psiISO 527-1,-3
Film Tensile Strength at Break, TD 65.0 MPa9430 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FISO 3146
Vicat Softening Point 72.0 °C162 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
 
Descriptive Properties
Processing MethodBlown film, sheet
Test Specimenfilm properties tested using 20µm thickness at 220°C, long stalk process, blow up ratio 4:1.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostalen ACP 9255 PLUS High Density Polyethylene (HDPE), Film Grade
LyondellBasell Luflexen hyPE 35P FA Polyethylene
LyondellBasell Hostalen ACP 9254 Plus High Density Polyethylene (HDPE), Film Grade
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications
Dow HDPE 25455N High Density Polyethylene

PEQT8457 / 220092

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.