MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound
Categories: Polymer; Thermoset; Bismaleimide (BMI); Carbon Fiber/Thermoset Composite

Material Notes: Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levels

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ISO 60
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Water Absorption 0.60 %0.60 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-1
Elongation at Break 0.60 %0.60 %ISO 527-1
Tensile Modulus 16.0 GPa2320 ksiISO 527-1
Flexural Strength 136 MPa19700 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Compressive Strength 132 MPa19100 psiISO 604
Charpy Impact, Notched 2.40 J/cm²11.4 ft-lb/in²ISO 179-1
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 275 °C527 °F
 
Descriptive Properties
ColorDark Grey
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
Sumitomo Bakelite KINEL® SK4525 S5A BMI Molding Compound
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin 4581 Astroquartz III

PVYNCN936 / 142711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.