MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Edinburg Plastics BCT505 PC/PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Appearance: Flame Retardant Colors

Processing Methods: Injection

Applications: Pump housings and Electrical switches

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792-91
Linear Mold Shrinkage 0.0080 - 0.014 cm/cm0.0080 - 0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 48.3 MPa7000 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Flexural Yield Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.07 GPa300 ksiASTM D790
Izod Impact, Notched 5.87 J/cm11.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C208 °FASTM D648
Flammability, UL94 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 243 °C450 - 469 °F
Middle Barrel Temperature 232 - 254 °C450 - 489 °F
Front Barrel Temperature 243 - 266 °C469 - 511 °F
Nozzle Temperature 249 - 271 °C480 - 520 °F
Melt Temperature 260 °C500 °F
Mold Temperature 54.0 - 77.0 °C129 - 171 °F
Drying Temperature 116 °C241 °F
Dry Time 4.00 - 12.0 hour4.00 - 12.0 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point >= -40.0 °C>= -40.0 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiLower is better
Screw Speed 40 - 70 rpm40 - 70 rpmLower is better

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® UT5205 PC/PBT Blend
Covestro Makroblend® UT3907 PC+PBT
A. Schulman Diamond DIAMALOY 527 PC/PBT Alloy
Edinburg Plastics CBI606 PC/PBT
Avient Edgetek® XT XT-100-CX01 PC+PBT

PEDIN010 / 183513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.