MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Silres® WH 80A Silicone Hybrid Emulsion
Categories: Polymer; Thermoset; Silicone

Material Notes: SILRES® WH 80A is a water reducible, solvent free, emulsion of a siloxane which can be used to increase beading and water repellency of cellulosic substrates. The modification of water reducible organic polymers such as alkyds or acrylic latexes with the SILRES® WH 80A will increase the water repellency and beading after exposure to UV radiation.

Special features:

  • Provide water repellency to cellulosic substrates
  • Provides excellent short term and long term beading
  • Low VOC before and after curing according to EPAmethod 24
  • Waterborne and easy to apply
  • UV stable and resistant to cracking, peeling and blistering
  • Retains color and gloss after weathering in coating formulations
Application: SILRES® WH 80A can be used as a clear penetrating sealer for cellulosic substrates and used as a modifier for water reducible or latex polymers.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³WSTM 3097
Solids Content 45 - 49 %45 - 49 %WSTM 3290
Viscosity <= 2000 cP<= 2000 cPWSTM 3001
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 212 °C>= 414 °FClosed cup
 
Descriptive Properties
Appearancemilky white emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-T80 + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Dow CE 8401 EMULSION
Wacker Wacker® UF 6 Lubricant
Metalon Products Metalon® HPS-021 Electrically Conductive Inks
Daikin NEOFLON® ND-1 FEP Dispersion, Translucent White

PWACK9589 / 205118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.