MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akrotek® PK-VM (4774) PK Conditioned
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: The renaissance of this polymer came about with an environmental program aimed at reducing greenhouse gases. The comonomer is CO (carbon monoxide), an industrial „waste” gas, which forms an unusual product when bonding with the polymer. The terpolymer, which forms the basis of most AKROTEK® PK formulations when using the monomers ethylene and propylene, currently has the greatest significance. AKRO-PLASTIC GmbH produces two product families from this base polymer (HM = normal flow and VM = very easy-flowing), based on the former portfolio of the Shell AG, from non-reinforced to high-glass-fibre-reinforced standards, from flame-retardant to carbon-fibre-reinforced custom grades

The characteristic properties of these properties include:

  • excellent dynamic resilience
  • good barrier properties
  • good tribological properties
  • high resistance to chemicals
  • good hydrolysis resistance
  • shorter cycle times
Application areas:
  • Industry
  • Automotive industry
  • Electronics/Electrical

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Moisture Absorption 0.80 - 0.90 %
@Temperature 70.0 °C
0.80 - 0.90 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi50 [mm/min]; ISO 527-2
Elongation at Break >= 200 %>= 200 %50 [mm/min]; ISO 527-2
Tensile Modulus 1.50 GPa218 ksi1 [mm/min]; ISO 527-2
Flexural Strength 70.0 MPa10200 psi2 [mm/min]; ISO 178
Flexural Modulus 1.50 GPa218 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akrotek® PK-HM (4773) PK Conditioned
Akro-Plastic Akrotek® PK-VM (4774) PK Dry
Akro-Plastic Akrotek® PK-HM (4773) PK Dry
Akro-Plastic Akrotek® PK-HM GF 15 (4707) PK Dry, 15% Glass Filled
Celanese Hostaform® C 9021 POM, Unfilled

PAKRO134 / 182721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.