MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type 430F Stainless Steel annealed bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Material Notes:

Key Words: UNS S43020, ASTM A314, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (51430F), DIN 1.4104, AFNOR Z 10 CF 17 (Fr), UNI X 10 CRs 17, JIS SUS 430 F, SS14 2383 (Sweden), ferritic, ISO 683/13 8a
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Hardness, Knoop 189189Converted from Brinell
Hardness, Rockwell B 8686Converted from Brinell
Hardness, Vickers 178178Converted from Brinell
Tensile Strength, Ultimate 550 MPa79800 psi
Elongation at Break 25 %25 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000610 ohm-cm0.0000610 ohm-cm
Magnetic Permeability 600 - 1100600 - 1100annealed condition at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 20.0 °C
5.78 µin/in-°F
@Temperature 68.0 °F
 11.2 µm/m-°C
@Temperature 250 °C
6.22 µin/in-°F
@Temperature 482 °F
 11.9 µm/m-°C
@Temperature 500 °C
6.61 µin/in-°F
@Temperature 932 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 24.9 W/m-K173 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 815 °C1500 °FContinuous Service
 870 °C1600 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 16 %16 %
Iron, Fe 81 %81 %
Manganese, Mn <= 1.25 %<= 1.25 %
Molybdenum, Mo <= 0.60 %<= 0.60 %Optional
Potassium, K <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S >= 0.15 %>= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 430F Stainless Steel
430 Stainless Steel annealed bar
AISI Type 316F Stainless Steel, annealed bar
304 Stainless Steel
430 Stainless Steel annealed sheet

MQ430B / 13129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.