Description: MTM110 series prepregs are high temperature resistant, inherently flame-retardant, cyanate ester matrices suitable for initial cure at 135°C (275°F). After a suitable post-cure, the glass transition temperature can be increased to a maximum of 330°C (626°F), thus allowing components to withstand short duration thermal spikes up to this temperature. MTM110 series autoclave processing prepregs have been specially developed for applications where extended room temperature out life is important. Features & Benefits: - 135°C (275°F) initial cure
- 30 days out life at 21° (70°F)
- Autoclave cure
- Good thermal durability up to 250°C (482°F) after post-cure
- Good dielectric properties for radar transparency
- Maximum Tg of 330°C (626°F); can withstand thermal spikes to 330°C (626°F)
- Inherently flame retardant, with low toxic gas and smoke generation
Product Variants: MTM110-5: For unidirectional prepregs MTA110-5: Film for bonding applicationsNote 1: Material: MTM110/Quartz 581 fabric; Cure: 3 hrs at 135°C (275°F), 6 bar (87 psi); Information provided by Cytec, subsequently acquired by Solvay. |