MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Devcon High-Performance Backing Compound Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Abrasion-Resistant System

Data provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0581 lb/in³
Viscosity 10320 cP10320 cPwith hardener
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9292ASTM D2240
Tensile Strength, Ultimate 53.00 MPa7687 psiASTM D638
Tensile Modulus 6.55 GPa950 ksiASTM D638
Flexural Yield Strength 79.3 MPa11500 psiASTM D790
Compressive Yield Strength 130.0 MPa18850 psiASTM D695
Adhesive Bond Strength 13.8 MPa2000 psiAdhesive tensile shear strength; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 121 °C250 °FOperating Temperature
Shrinkage 0.060 %0.060 %During Cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Processing Temperature 21.1 °C70.0 °F
Pot Life 56.0 min
@Temperature 23.9 °C
56.0 min
@Temperature 75.0 °F
 
Descriptive Properties
Coverage per 20.3 lb.347 in²
Mix Ratio by Volume9.95 to 1resin:hardener
Mix Ratio by Weight100 to 5.94resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 8504-5 One-Component Epoxy
Overview of materials for Epoxy Adhesive
BCC Products BC 7009-1 Epoxy Casting
Armstrong A-1/V Epoxy Adhesive
Aremco Aremco-Bond™ 631 High Performance Epoxide

PITWX24 / 48511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.