MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Cogegum® GFR/370 Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission. This material complies with RoHS requirements. Standard complying - EN 50363-6 EM8, EM10; EN 50264 EM101..104; IEC 60092 SHF2; VDE 0207 HM3

Additional Information: Tests reported are performed on pressed or extruded specimens, added with 3% of Catalyst CT/2-MD UV and crosslinked in hot water at 95°C for 6 hours Coloring - EVA or PE based masterbatches added at 1.2-1.5% by weight; in order to avoid scotching problems during processing, predrying of colour masterbatch is suggested if moisture absorption occurred during storage (4-6 hours at 50-60°C). Storage - The product must be stored under the following conditions: -- closed and unteared bags -- ambient temperature not exceeding 35°C -- avoid direct exposure to sunlight and weathering - Product alterations could occur due to extended period of storage - Shelf life: 6 months - Solvay Specialty Polymers accepts no liability of any kind in case the above mentioned conditions are not fulfilled. Packaging - 25 kg moisture-resistant bags on 1375 kg pallet - 1000 kg carton box

Extrusion Notes: Processing - COGEGUM® GFR/370 pregrafted base must be added with Catalyst CT/2-MD UV masterbatch to promote curing. Catalyst dosage is 3% by weight and blending must be done just before using (2-3 hours max.), preferably in the extruder hopper. Catalyst doesn't need any predrying if stored in dry conditions in the original closed bags; in case, predrying can be made at 50-60°C for 4-8 hours - The pregrafted base compound is sensible to moisture; open bags must be used within 4 hours. Pregrafted base cannot be predried Extrusion equipment - standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 25 L/D ratio are suggested), and an adequate barrel thermoregulation - don't use screw thermoregulation - filter net: none - compression tools suggested Curing - by immersion in hot water at 60-70°C - by exposure in ambient, crosslinking time depends on ambient temperature and relative humidity - in all cases curing time depends on insulation thickness; for 0.7-1.2 mm wall thickness 3-6 hours are generally necessary in case of forced curing in hot water

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
ESCR 10% Igepal® >= 1000 hour
@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour
@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded; ASTM D1693
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
without Catalyst MB addition; Internal Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ISO 868
Tensile Strength at Break 12.0 MPa1740 psiIEC 60811
Elongation at Break 150 %150 %IEC 60811
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 290 °C554 °FTemperature Index (Burning); NES 715
Oxygen Index 30 %30 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °FCollar Temperature
Zone 1 130 - 150 °C266 - 302 °F
Zone 2 130 - 150 °C266 - 302 °F
Zone 3 140 - 160 °C284 - 320 °F
Zone 4 140 - 160 °C284 - 320 °F
Die Temperature 160 - 180 °C320 - 356 °F
Head Temperature 150 - 170 °C302 - 338 °F
 
Descriptive Properties
1N NaOH Solution Immersion Test, 23°C, 168 hr-3% Change in Tensile StrengthIEC 60811
 -30% Change in Tensile ElongationIEC 60811
1N Oxalic Acid Immersion Test, 23°C, 168 hr-7% Change in Tensile StrengthIEC 60811
 -8% Change in Tensile ElongationIEC 60811
AvailabilityAsia Pacific
 Europe
 North America
Bending TestNo cracks-40°C; IEC 60811
Calorific Potential15.5 MJ/kgISO 1716; Upper (gross)
Corrosive Gas in Smoke< 10.0 µS/mmConductivity IEC 60754-2
 pH > 4.30
FeaturesCrosslinkable
 Flame Retardant
 Fuel Resistant
 Halogen Free
 Low Smoke Emission
 Low Toxicity
 Oil Resistant
 Self Extinguishing
GenericPolyolefin, Unspecified
Halogenidric Acid Emissions< 0.10%
Hot Pressure Test< 50%125°C; max penetration, K=1; IEC 60811
Hot Set (%)0200°C, Permanent elongation after cooling; 20 N/cm²
 40200°C, Elongation under load
IRM 902 Oil Immersion Test, 100°C, 168 hr-14IEC 60811, %Change in Tensile Elongation
 -18IEC 60811, %Change in Tensile Strength
IRM 902 Oil Immersion Test, 121°C, 18 hr-27Change in Tensile Strength
 -8IEC 60811, %Change in Tensile Elongation
IRM 903 Oil Immersion Test, 100°C, 168 hr-12IEC 60811, %Change in Tensile Strength
 -17IEC 60811, %Change in Tensile Elongation
IRM 903 Oil Immersion Test, 70°C, 168 hr-21IEC 60811, %Change in Tensile Elongation
 -8IEC 60811, %Change in Tensile Strength
Mechanical Properties After Aging in Air Bomb, 0.55 MPa, 127°C, 40 hr19IEC 60811, %Change in Tensile Strength
 -24IEC 60811, %Change in Tensile Elongation
Mechanical Properties After Aging in Air Oven, 135°C, 168 hr16IEC 60811, %Change in Tensile Strength
 -24IEC 60811, %Change in Tensile Elongation
RoHS ComplianceRoHS Compliant
UsesCable Jacketing
 Wire & Cable Applications
Water Absorption (mg/cm²)< 1.00100°C; 24 hr; IEC 60811

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidiemme® G/220 Thermoset Elastomer (TSE)
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/320 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/340-HP Polyolefin
Syensqo (Solvay Specialty Polymers) Polidiemme® G/430 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/380 Polyolefin

PSOL8Y7633 / 135696

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.