MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Portland Cement
Categories: Ceramic; Concrete

Material Notes: Portland cement (Type I) paste with no aggregate prepared with a water/cement ratio of 0.35:1 and cured 28 days.

This data comes from a study that examined the effect of silica fume on Portland cement pastes. A total of four data sheets are in MatWeb from this study.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.01 g/cc0.0726 lb/in³
Porosity 2.32 %2.32 %Air Void Content
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.910 MPa132 psi
Elongation at Break 0.0041 %0.0041 %In Tension
Tensile Modulus 11.2 GPa1620 ksi
Compressive Strain at Break 1.72 %1.72 %
Compressive Strength 57.9 MPa8400 psi
Compressive Modulus 2.92 GPa424 ksi
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.736 J/g-°C0.176 BTU/lb-°F
Thermal Conductivity 0.530 W/m-K3.68 BTU-in/hr-ft²-°F
Shrinkage 0.0498 %0.0498 %Upon drying

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Granite
Concrete, Highstrength
Portland Cement with Untreated Silica Fume
Concrete, Lightweight
Portland Cement with Treated Silica Fume

CLAC200 / 1471

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.