MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese VECTRA MLX4243 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: High heat resistant, mineral filled LCP material with high flow. Material has silver metallic appearance for use in aesthetic metallic effect applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.5 %2.5 %5mm/min; ISO 527-2/1A
Tensile Modulus 12.5 GPa1810 ksi50mm/min; ISO 527-2/1A
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 13.2 GPa1910 ksiISO 178
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 332 °C630 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 130 °C176 - 266 °Fcavity
Zone 1 315 - 325 °C599 - 617 °F
Zone 2 325 - 335 °C617 - 635 °F
Zone 3 330 - 345 °C626 - 653 °F
Zone 4 335 - 350 °C635 - 662 °F
Die Temperature 335 - 345 °C635 - 653 °F
Melt Temperature 335 - 345 °C635 - 653 °F
Drying Temperature >= 150 °C>= 302 °F
Dry Time 6.00 hour6.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 50.0 - 150 MPa7250 - 21800 psi
 
Descriptive Properties
Injection speedvery fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA A950 LCP, Unfilled
EMS-Grivory Grilamid® L 20 W 20 PA12
RTP Company RTP 3400-3 Liquid Crystal Polymer (LCP), Unfilled
Celanese Vectra® C115 Liquid Crystal Polymer (LCP), 15% Glass Reinforced
Celanese Zenite® 5145L BK010 LCP

PHCQ517 / 178972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.