MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for automotive valve housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.80 - 1.2 %0.80 - 1.2 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.3 - 5.3 %4.3 - 5.3 %ISO 62
Viscosity Measurement 130130ISO 307
Linear Mold Shrinkage 0.0033 cm/cm0.0033 in/inrestricted
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  40.0 MPa
@Strain 2 %,
Temperature 150 °C
5800 psi
@Strain 2 %,
Temperature 302 °F
5mm/min
 50.0 MPa
@Strain 2 %,
Temperature 100 °C
7250 psi
@Strain 2 %,
Temperature 212 °F
5mm/min
 100 MPa
@Strain 2 %,
Temperature 80.0 °C
14500 psi
@Strain 2 %,
Temperature 176 °F
5mm/min
 110 MPa
@Strain 1 %,
Temperature 60.0 °C
16000 psi
@Strain 1 %,
Temperature 140 °F
5mm/min
 120 MPa
@Strain 3 %,
Temperature 80.0 °C
17400 psi
@Strain 3 %,
Temperature 176 °F
5mm/min
 160 MPa
@Strain 2 %,
Temperature 60.0 °C
23200 psi
@Strain 2 %,
Temperature 140 °F
5mm/min
 175 MPa
@Strain 1 %,
Temperature 23.0 °C
25400 psi
@Strain 1 %,
Temperature 73.4 °F
5mm/min
 200 MPa
@Strain 2 %,
Temperature 23.0 °C
29000 psi
@Strain 2 %,
Temperature 73.4 °F
5mm/min
Tensile Strength, Yield 210 MPa30500 psi50 mm/min; ISO 527-1/-2
Tensile Stress at Strain  60.0 MPa
@Strain 6.0 %,
Temperature 150 °C
8700 psi
@Strain 6.0 %,
Temperature 302 °F
5mm/min
 65.0 MPa
@Strain 9.0 %,
Temperature 150 °C
9430 psi
@Strain 9.0 %,
Temperature 302 °F
5mm/min
 75.0 MPa
@Strain 6.0 %,
Temperature 100 °C
10900 psi
@Strain 6.0 %,
Temperature 212 °F
5mm/min
 80.0 MPa
@Strain 9.0 %,
Temperature 100 °C
11600 psi
@Strain 9.0 %,
Temperature 212 °F
5mm/min
 125 MPa
@Strain 5.0 %,
Temperature 80.0 °C
18100 psi
@Strain 5.0 %,
Temperature 176 °F
5mm/min
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 12.0 GPa1740 ksiISO 527-1/-2
 5.00 GPa
@Temperature 140 °C
725 ksi
@Temperature 284 °F
ISO 527
 9.00 GPa
@Temperature 80.0 °C
1310 ksi
@Temperature 176 °F
ISO 527
 12.0 GPa
@Temperature 0.000 °C
1740 ksi
@Temperature 32.0 °F
ISO 527
 12.0 GPa
@Temperature 40.0 °C
1740 ksi
@Temperature 104 °F
ISO 527
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
 2.00e+9 ohm-cm
@Temperature 140 °C
2.00e+9 ohm-cm
@Temperature 284 °F
IEC 60093
 6.00e+10 ohm-cm
@Temperature 120 °C
6.00e+10 ohm-cm
@Temperature 248 °F
IEC 60093
 1.00e+13 ohm-cm
@Temperature 100 °C
1.00e+13 ohm-cm
@Temperature 212 °F
IEC 60093
 1.00e+15 ohm-cm
@Temperature 80.0 °C
1.00e+15 ohm-cm
@Temperature 176 °F
IEC 60093
 5.00e+15 ohm-cm
@Temperature 60.0 °C
5.00e+15 ohm-cm
@Temperature 140 °F
IEC 60093
 5.00e+15 ohm-cm
@Temperature 20.0 °C
5.00e+15 ohm-cm
@Temperature 68.0 °F
IEC 60093
 1.00e+16 ohm-cm
@Temperature 40.0 °C
1.00e+16 ohm-cm
@Temperature 104 °F
IEC 60093
Dielectric Constant 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 - 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
27.8 - 33.3 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
CTE, linear, Transverse to Flow 15.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity 1.30 J/g-°C0.311 BTU/lb-°F
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FDIN 52612
Melting Point 295 °C563 °FDIN 53765
Maximum Service Temperature, Air 135 °C275 °Ffor 50% loss of tensile strength after 20000hr
 160 °C320 °Ffor 50% loss of tensile strength after 5000hr
 270 °C518 °F
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 330 °C590 - 626 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection-molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned)
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)

PBASG0290 / 131923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.