MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Petra® 130 BK-112 30% Glass Filled PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength and stiffness at elevated temperatures. It also has good chemical resistance and dimensional stability, and adequate ductility for most applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Viscosity Measurement 0.550.55Inherent Viscosity
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM Test
Tensile Strength at Break 145 MPa21000 psi0.2 in/min; ASTM Test
 54.0 MPa
@Temperature 120 °C
7830 psi
@Temperature 248 °F
ISO Data
 211 MPa
@Temperature -40.0 °C
30600 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Ultimate 145 MPa21000 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
 3.0 %3.0 %0.2 in/min; ASTM Test
 2.3 %
@Temperature -40.0 °C
2.3 %
@Temperature -40.0 °F
ISO Data
 4.0 %
@Temperature 120 °C
4.0 %
@Temperature 248 °F
ISO Data
Tensile Modulus 10.2 GPa1480 ksi1mm/min; ISO 527
Flexural Strength 230 MPa33400 psiASTM Test
Flexural Modulus 8.25 GPa1200 ksiISO Data
 8.76 GPa1270 ksiASTM Test
Izod Impact, Notched 0.950 J/cm
@Thickness 3.17 mm
1.78 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²ISO Test
 8.50 kJ/m²
@Temperature -40.0 °C
4.04 ft-lb/in²
@Temperature -40.0 °F
ISO Test
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 0.850 J/cm²
@Temperature -30.0 °C
4.05 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
12.8 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 245 °C473 °F10 K/min
 245 °C473 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 235 °C455 °FASTM Test
 240 °C464 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75
 215 °C419 °FASTM Test
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 115 °C239 °FInjection molding
 
Descriptive Properties
ColorBK-112
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Petra® 130 FR 30% Glass Filled PET
BASF Petra® 130 30% Glass Filled PET
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced
Bamberger Polymers Bapolene® 82 Polyethylene Terephthalate
BASF Petra® 110 BK-112 15% Glass Filled PET

PBASF9017 / 84781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.