System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
NSF Standard 61 Certified
Available in Americas, Europe, Middle East, Africa, India and Asia
Information provided by Lubrizol
Lubrizol acquired the Isoplast product line from Dow in 2009.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.20
g/cc
1.20
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
62.1
MPa
9000
psi
ASTM D638
Tensile Strength, Yield
68.9
MPa
10000
psi
ASTM D638
Elongation at Break
90 %
90 %
ASTM D638
Elongation at Yield
9.0 %
9.0 %
ASTM D638
Tensile Modulus
1.79
GPa
260
ksi
ASTM D638
Flexural Strength
89.6
MPa
13000
psi
ASTM D790
Flexural Modulus
2.21
GPa
320
ksi
ASTM D790
Izod Impact, Notched
1.60
J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
3.00
ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
5.34
J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
10.0
ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Dart Drop, Total Energy
34.0
J
@Temperature -28.9 °C
25.1
ft-lb
@Temperature -20.0 °F
ASTM D3763
45.0
J
@Temperature 22.8 °C
33.2
ft-lb
@Temperature 73.0 °F
ASTM D3763
Thermal Properties
Metric
English
Comments
CTE, linear
66.6
µm/m-°C
@Temperature 20.0 °C
37.0
µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
127
°C
260
°F
unannealed; ASTM D648
143
°C
290
°F
annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
116
°C
240
°F
unannealed; ASTM D648
138
°C
280
°F
annealed; ASTM D648
Vicat Softening Point
144
°C
292
°F
ASTM D1525
Processing Properties
Metric
English
Comments
Melt Temperature
238
-
260
°C
460
-
500
°F
Mold Temperature
93.0
-
121
°C
199
-
250
°F
Drying Temperature
127
-
138
°C
261
-
280
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
PDOW1393 / 30611
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.